Chen Zongping, Zheng Wei, Zhou Chunheng, Xue Jianyang. TEST OF STEEL REINFORCED RECYCLED AGGREGATE CONCRETE AXIAL COMPRESSION SHORT COLUMNS AFTER HIGH TEMPERATURE[J]. INDUSTRIAL CONSTRUCTION, 2014, 44(11): 32-38. doi: 10.13204/j.gyjz2001411006
Citation: Chen Zongping, Zheng Wei, Zhou Chunheng, Xue Jianyang. TEST OF STEEL REINFORCED RECYCLED AGGREGATE CONCRETE AXIAL COMPRESSION SHORT COLUMNS AFTER HIGH TEMPERATURE[J]. INDUSTRIAL CONSTRUCTION, 2014, 44(11): 32-38. doi: 10.13204/j.gyjz2001411006

TEST OF STEEL REINFORCED RECYCLED AGGREGATE CONCRETE AXIAL COMPRESSION SHORT COLUMNS AFTER HIGH TEMPERATURE

doi: 10.13204/j.gyjz2001411006
  • Publish Date: 2014-11-15
  • In order to reveal the axial compression behavior of steel reinforced recycled aggregate concrete ( SRRAC) columns after high temperature,18 specimens were designed for monotonic loading experiment after high temperature, and five varying parameters were considered,which were the high temperature,the constant temperature time,the cover thickness,the steel ratio and the stirrup ratio. The failure processes and forms of specimens at different temperatures were observed,the percentage of mass decrement,load-displacement curves,residual bearing capacity, and other important data were obtained. And the effecting law of each changing parameters on the SRRAC columns’ mechanical behavior after high temperature was analyzed. Results showed that the failure mode of SRRAC columns after high temperature was similar to that at normal temperature. The SRRAC columns after high temperature had certain deformation performance after ultimate load,but the axial rigidity and residual bearing capacity of specimens were reduced compared with that at normal temperature. The strength of the specimens after high temperature was reduced by 13% to 50%,which was reduced by 32% to 42% at 600 ℃.
  • loading
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Article Metrics

    Article views (107) PDF downloads(44) Cited by()
    Proportional views
    Related

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return