MECHANICAL PERFORMANCES OF HRB500A AND HRB500C CORROSION RESISTANT REBARS WITH INDIRECT BUTT SPLICES IN SINGLE SIDE WELDING
-
摘要: 为推进耐蚀钢筋的应用,揭示焊接耐蚀钢筋的力学性能,采用工程实践中常用的单面帮条焊的焊接方法,在优化焊接工艺参数的基础上,分别对耐蚀钢筋HRB500a和HRB500c的ϕ16、ϕ25和ϕ32三种典型规格的钢筋进行焊接,分析接头的微观组织及力学性能等,研究其可焊性及接头焊接性能。试验结果表明:选用合适的焊接材料和焊接工艺,耐蚀钢筋HRB500a和HRB500c采用单面帮条焊均能够得到焊接性能良好的焊接接头。Abstract: To promote the application of corrosion resistant rebars of high performances and reveal the mechanical performances, based on the optimization of welding parameters, the welding process of indirect butt splices in single side welding applied widely in practices was adopted and the welded specimens for three specification rebars ϕ16, ϕ25 and ϕ32 of HRB500a and HRB500c were prepared. The microstructure, mechanical properties of splices of being welded were tested and measured.The test results showed that both steels of HRB500a and HRB500c had good welding performances in cases of reasonable welding rods and welding processes with indirect butt splices in single side welding.
-
艾志勇.新型合金耐蚀钢筋的腐蚀行为及耐蚀机制[D].南京:东南大学,2017. 杨忠民,陈颖,王慧敏. 高强耐蚀钢筋[C]//2009全国建筑钢筋生产、设计与应用技术交流研讨会会议论文集.北京:中国金属学会,2009:138-142. 林雪君.福建省耐腐蚀钢筋产品的研发与应用[EB/OL].2018-01-30. https://gc.mysteel.com/18/0130/16/81ED059BC73C3EAE.html. 艾志勇,孙伟,蒋金洋.低合金耐蚀钢筋锈蚀研究现状及存在的问题分析[J].腐蚀科学与防护技术,2015,27(6):525-536.
点击查看大图
计量
- 文章访问数: 108
- HTML全文浏览量: 8
- PDF下载量: 1
- 被引次数: 0