钢板混凝土板平面外弯剪性能试验研究
doi: 10.13204/j.gyjz2001412004
EXPERIMENTAL STUDY OF OUT-PLANE BENDING SHEAR BEHAVIOR OF STEEL PLATE REINFORCED CONCRETE SLAB
-
摘要: 对5片剪跨比范围在2~5、距厚比为100和150的钢板混凝土板进行简支单点加载的平面外抗剪性能试验。试验结果表明:钢板混凝土板的破坏形式与钢筋混凝土结构类似;栓钉的间距对钢板混凝土(简称“SC”)板的刚度有很大影响;随着剪跨比的增大,抗剪承载力下降,试件破坏呈现脆性破坏;当试件截面高度增加时,试件破坏形式为剪切破坏。同时采用ACI 349和JEAG 4618对试件弯曲承载力和抗剪承载力进行计算,计算值与试验值吻合较好。Abstract: It was conducted simply supported single point load-out of plane shear performance tests for five specimens of steel plate reinforced concrete slab,whose shear-span ratio was in the range of 2 ~ 5,and the distance-thickness ratios of steel concrete slab and steel plate were 100 and 150. The test results show that damage in the form of a concrete slab with steel reinforced concrete structure is similar. Spacing of studs has a great impact on the SC board stiffness; With the shear span ratio increases,the shear capacity is decreased,and the specimen damage is a brittle failure; highly when the height of specimen section is increased,the specimen damage is in the form of cut destruction. While using ACI 349 and JEAG 4618 to calculate the bending bearing capacity and shear capacity of the specimen,the calculated and experimental values are in good agreement.
点击查看大图
计量
- 文章访问数: 155
- HTML全文浏览量: 10
- PDF下载量: 162
- 被引次数: 0